Nanomaterials are not new. The catalyst, carbon black, sol, fumed oxide and pigment industries have already commercialized several simple oxide nanopowders, nanoscale dispersion products and nanoparticle manufacturing processes that are an integral part of today's ceramic industry and the global economy.
What is new in the developing nanomaterials industry is the emergence of low-cost, high-volume, novel processes and processing innovations, which offer complex compositions with a level of precision and characteristics that were, in the past, either too difficult to achieve or too expensive to be commercially useful.
The continued development of processing technologies, the availability of better instruments to measure quality and features at ever-shrinking dimensions, the integration of computer-aided manufacturing, and a market demand for materials innovation is fueling the growth of nanomaterials and related nanotechnologies. Combined with the expertise that already resides in industries such as catalysts, pigments and fumed silica, nanomaterials are beginning to offer a foundation for innovative, value-added ceramic products.

To be commercially useful, nanoscale materials must possess certain characteristics. Table 1 lists some of the key properties for nanomaterials used in value-added and technology-intensive applications, such as those in the ceramic industry, as well as electronics, displays, energy devices, magnetics, dielectrics, coatings, additives, catalysts, multilayered devices, pigments, security and plastics.
Attrition methods attempt to break coarse, micron-sized particles into smaller particles by applying directed energy, such as milling. Some teams are exploring ways to perform the milling in a carefully controlled thermal, shear and chemical environment, and other teams are exploring the use of ultrasound energy. While appropriate for certain applications, these techniques have been reported to yield a product that is contaminated with the media or vessel that is used to break the coarse particles. Cost, yield and scalability are other issues that remain to be addressed with attrition methods.

Vapor methods first create a vapor comprising atoms and atomic clusters, followed by condensation and quenching of nanoparticles. The benefit of these processes is the diverse range of compositions they can achieve. However, in some versions of this approach, the need for high temperatures can result in higher energy costs, and it can also cause agglomeration and purity issues with some materials. If the quench is accomplished by adding coolants, the raw material and separation costs become higher. In certain cases, vapor methods tend to produce higher particle sizes for compositions (such as titanium oxide) with a very high refractive index and emissivity. Additionally, certain methods of feeding precursors and achieving higher temperatures (e.g., electrical energy) can, in some cases, limit the flexibility and scalability of the process.
The combustion product stream is further heated in a plasma to achieve peak temperatures greater than 3000 K (4940ºF) at supersonic velocities. The vapor is then cooled, which leads to nucleation of nanoscale powders. Thereafter, the powder-containing gas stream is quenched at near-sonic to supersonic velocities using a Joule-Thompson expansion step. The sonic quenching reduces collisions between the particles and produces free-flowing, non-agglomerated nanopowders, which are then continuously harvested.
If solid raw materials such as commercially available micron-sized ceramic powders are used, these are fed directly into a DC plasma to create a vapor comprising various metals. Thereafter, the nucleation and quench of nanoparticles is performed as explained previously.

The process has been used to produce more than 200 compositions, including simple oxides, complex doped or multi-metal oxides, non-oxides, and metals in particle sizes as small as 2 to 10 nanometers, coarser 20 to 40 nanometers, 60 to 80 nanometers, and submicron particles. Nanoscale materials produced from this process have been dispersed successfully in water and solvents at high loadings. The process can be used to produce stoichiometric compositions, such as Al2O3, stabilized ZrO2, BaFe2O4 and SiO2, as well as non-stoichiometric compositions, such as BaFe1.5Ox and SiOxNy. The flexibility of the process has enabled systematic nanoscale material discovery and optimized material performance.
The volume and pricing of nanomaterials is already in a range that makes a number of commercial applications economically compelling. With the increasing availability of nanomaterials and the associated processing know-how, a commercial world based on nanotechnology is beginning to emerge. c
About the Author
Tapesh Yadav is chairman and chief executive officer of NanoProducts Corp., which he founded in 1994. Yadav has a doctorate in chemical engineering from the Massachusetts Institute of Technology and a minor in finance from the Sloan School of Management. He has more than 12 years of experience with a wide range of nanomaterials and related nanotechnology applications, and has been awarded more than 45 U.S. patents on nanomaterials and related nanotechnology applications.
Fore More Information For more information about nanoscale materials, contact NanoProducts Corp., 14330 Longs Peak Court, Longmont, CO 80504; (970) 535-0629; fax (970) 535-9309; e-mail staff@nanoproducts.com; or visit www.nanoproducts.com.
FOOTNOTE:
*The Joule-QuenchTM technology, a process patented by NanoProducts Corp.2
References
1. Gammon, D. Nature, Vol. 405, No. 899, 2000; Gleiter, H. Acta Mater., Vol. 48, No. 1, 2000; and Valiev, R. Nature, Vol. 419, No. 887, 2002.
2. U.S. Patent Nos. 6652967, 6641775, 6610355, 6344271, 6228904, 5984997, 5851507 and 5788738.