Orton Ceramic Foundation: Dilatometer Software
September 29, 2000
The company’s dilatometer software for Windows® is detailed in a four-page color brochure. Key features of the software include logical organization, streamlined design and multiple user options, including the ability to export ASCII files to other software programs. The software also enables users to graph up to six runs; change X or Y axis values to plot PLC, DCE or ACE against time or temperature; determine transition temperature or glass softening points; and calculate coefficient of expansion for any temperature range. With samples and explanations, the brochure details the software’s data analysis, data set-up and data review screens. Special and print options are also explained.