Available from Pred Materials International, Inc., BSP-80 is a new specially treated expanded graphite powder additive for MgO-C (mag-carbon) refractory brick.
Available from Pred Materials International, Inc. and made in Japan by Chuetsu Graphite Works, BSP-80 is a new specially treated expanded graphite powder additive for MgO-C (mag-carbon) refractory brick. The powder, which has been developed to increase high-heat shock resistance, offers improved molding and forming, improved physical strength of MgO-C products, reduced binder consumption and improved spalling resistance.
For complete technical information, call (212) 286-0068, fax (212) 286-0072, e-mail Predmatsp@aol.com or visit http://www.predmaterials.com.