Premier Mill has introduced a new brochure detailing its models 50 and 2000 laboratory dispersators. The model 2000 produces consistently repeatable dispersions through a newly designed digital speed controller, providing improved motor performance. This high-speed unit ensures constant mixing speed regardless of product changes in viscosity, temperature or other variables. The unit breaks up agglomerates, reduces particle size, overcomes surface forces and speeds up chemical reactions involving insoluble materials. The economical model 50 is designed for lab applications requiring the power of the model 2000, but with a different control unit.
For additional information, call (610) 779-9500, fax (610) 779-9666, e-mail pmsales@lightnin.spx.com or visit http://www.premiermill.com .