Rath Opens New Plant in Georgia (7/25/06)
July 26, 2006
Austria-based Rath Group AG has opened a new refractory plant in Milledgeville, Ga. Operated by Rath Refractories, Inc., the plant produces alumina-silica brick and shapes for critical applications in the energy and chemical markets. The Milledgeville site was chosen for its proximity to local raw materials, customers and the port of Savannah. The greenfield plant features state-of the-art batching, mixing, pressing and firing equipment.