RIS Group announced the offering of it's new line of refractory products.
Refractory & Industrial Supply Group, Inc. (RIS Group), a division of Diversified Thermal Solutions, Inc. (DTS), recently announced the offering of its new line of refractory monolithics and brick products under the newly launched RIS Group brand name, which is in keeping with the long-term business strategy to become a full service provider of refractory products. RIS Group offers a complete line of refractory monolithics (non-brick materials) and firebrick products, including high alumina/low cement castables (RISFLOW 60 LC), and fused or vitreous silica brick products (RISIL).
For more information, call (901) 365-6632.