Sauereisen manufactures a diverse line of electrically insulating inorganic cements, including over 20 different air-, hydraulic- and chemical-setting products. Offering continuous high-temperature service of up to 3000¿F and dielectric strengths surpassing 100 volts/mil, these cements are particularly well suited for electrical and general assembly, embedding, insulating, sealing, coating and potting.