Simultaneous Thermal Analyzer
July 30, 2000
Netzsch Instruments Inc.
This company has introduced the new simultaneous thermal analyzer STA 409 PC Luxx® for true heat-flux DSC/DTA-TGA to 1550°C. The new system determines mass changes (thermogravimetry), characteristic temperatures and enthalpy changes (differential scanning calorimetry) on one sample in one measurement. Exchangeable sensors and a range of crucibles are available to accommodate a variety of applications.