Structure of a colloid gel. (Illustration by Paddy Royall, University of Bristol.)
Imagine
a plane with wings made out of glass. Thanks to a breakthrough in understanding
the nature of glass by scientists at the University of Bristol, such a
craft could become a possibility. Despite its solid appearance, glass is
actually a “jammed” state of matter that moves very slowly. Like cars in a
traffic jam, atoms in a glass can’t reach their destination because the route
is blocked by their neighbors. As a result, glass never quite becomes a
“proper” solid.
For more than 50 years, scientists have tried to understand just what glass is.
Work so far has concentrated on trying to understand the traffic jam, but Paddy
Royall, Ph.D., from the University of Bristol, with colleagues in Canberra and
Tokyo, has recently shown that the problem really lies with the destination.
Studying Structure
The team has discovered that glass “fails” to
be a solid due to the special atomic structures that form in a glass when it
cools (i.e., when the atoms arrive at their destination). “Some materials
crystallize as they cool, arranging their atoms into a highly regular pattern
called a lattice,” said Royall. “But although glass ‘wants’ to be a crystal, as
it cools the atoms become jammed in a nearly random arrangement, preventing it
from forming a regular lattice. Back in the 1950s, Sir Charles Frank in the
Physics Department at Bristol
University suggested that
the arrangement of the ‘jam’ should form what is known as an icosahedron, but
at the time he was unable to provide experimental proof. We set out to see if
he was right.”
The problem is you can’t watch what happens to atoms as they cool because they
are just too small. Using special particles called colloids that mimic atoms
but are just large enough to be visible using state-of-the-art microscopy,
Royall cooled some down and watched what happened.
What he found was that the gel these particles formed also “wants” to be a
crystal, but it fails to become one due to the formation of icosahedra-like
structures, exactly as Frank had predicted 50 years ago. It is the formation of
these structures that underlies jammed materials and explains why a glass is a
glass and not a liquid, or a solid.
Potential Metallic Glasses
Knowing the structure formed by atoms as a
glass cools represents a major breakthrough in our understanding of meta-stable
materials and will allow further development of new materials such as metallic
glasses. Metals normally crystallize when they cool. Unfortunately, stress
builds up along the boundaries between crystals, leading to metal failure.
The world’s first jetliner, for example, the British-built De Havilland Comet,
fell out of the sky due to metal failure. If a metal could be made to cool with
the same internal structure as a glass and without crystal grain boundaries, it
would be less likely to fail. Metallic glasses could be suitable for a whole
range of products that need to be flexible, including aircraft wings, golf
clubs and engine parts.
The
university’s website at www.bristol.ac.uk offers additional information.