This company has added an extrusion process to its current manufacturing methods of ceramic tubular capacitors. Adding this process reportedly enhances the company’s design flexibility with an increased custom product offering. The company can now produce sizes of up to 1 in. in length, as well as diameters of ½ in. and larger. Extruded ceramic tubular capacitors can be used for applications such as EMI filtering for multi-pin connectors, RFI suppression and circuit protection.