Superconductive Components, Inc. recently announced the introduction of two magnesium diboride (MgB2) products. MgB2 was recently discovered to be a superconductor and is expected to be used in a number of superconductor applications -- in particular microelectronics such as ultrahigh-performance analog-to-digital converters in all-digital software-defined radio systems for wireless applications. MgB2 is considered to be closer to the ideal material for superconducting electronics than any others discovered to date.
Additional information is available at
http://www.superconductivecomp.com.