An environmentally friendly plasticizer is now being offered by The Tape Casting Warehouse Division of Richard E. Mistler, Inc. The plasticizer, designated as S-2075, is a triethylene glycol-based material that is reportedly non-hazardous to humans and the environment. It has been evaluated to be a direct substitute for commonly used phthalate-based plasticizers in PVB tape casting systems.