Thermo ARL has announced the availability of its new powder XRD system, the ARL X-TRA. Combining 25 years of XRD experience and engineering excellence, the system offers the cost effective solution for high quality powder diffraction applications. Built around a vertical goniometer, this instrument offers the most convenient geometry for handling powder samples by facilitating the sample preparation, sample changer options and use of specialized sample holders. In order to optimize experimental conditions, the goniometer features removable dual Soller slits and continuous variable micrometer-controlled slits for adjusting the width of both the incident and diffracted beams.
For additional information, call (313) 271-5760 or visit http://www.thermoarl-us.com.