TSI(R) Inc. recently announced the introduction of its new PSD 3603 particle size distribution analyzer, designed and built to meet the rigorous demands of industrial powder and pharmaceutical manufacturers. The new analyzer is a powerful tool for characterizing dry powders and medical aerosols according to particle size. It measures particles in the range of 0.2 to 700 micrometers in diameter using an aerodynamic time-of-flight technique. Key features include 21 CFR 11-compliant software, high-resolution measurements, fast setup and cycle time, complete dispersion without milling, and repeatable results.
For more information, call (800) 677-2708 or (651) 490-2811, or e-mail powder@tsi.com .