A new line of superior performance diamond grinding wheels is available from Turner Tooling Co., Inc. A new bond development greatly reduces grinding forces and increases stock removal rates. The new bond also offers very free cutting, resulting in reduced wheel wear and extended wheel life. Test grinding on sintered SiC, Al SiC, SiNi, CVD SiC and B4C boron carbide have generated G-ratios ranging from 400 to over 800. ID, OD, and face and disc wheels are available.