Pantelejmonovskij has worked with Sacmi Imola to implement its development strategies since 1997.
JSC Panteleymonovka Refractory Plant is reportedly one of the Ukrainian market’s leading refractory product manufacturers. Equipped with high-output facilities, the company focuses on innovation, producing ever-better performing products and implementing sales and product policies that ensure an ever-stronger presence on the home market. Pantelejmonovskij has worked with Sacmi Imola to implement its development strategies.
The industrial partnership with Sacmi began in 1997 with the delivery of two 1600-ton presses. The partnership was strengthened in 2001 with the delivery of a 2500-ton press and in 2005 with a 1000-ton press. This synergy continued in 2007 when Pantelejmonovskij chose the Sacmi Group once again, this time signing a contract for the installation of a new PHR1600 press.