Micron Diamond-plus from Warren/Amplex Superabrasives was designed to avoid causes of variation inherent in particle manufacturing. Through precise and non-traditional control of the grading process, Warren/Amplex dramatically reduces adjusted center grading effects. While traditional product specifications usually confine product tolerances to mean volume (Mv), d10 and d90, or in some cases d95 of the distribution, the Micron Diamond-plus product line provides tighter limits on the d50 (median), d10 and d99 of the distribution. This approach yields a particle distribution that has a higher degree of accuracy and repeatability for the median of the distribution (d50), fine end (d10) and coarse end (d99). For more information, call (800) 368-5155, e-mail ron.a.abramshe@saint-gobain.com or visit www.warrenamplex.com.