Ceramic Industry

Zinsser: Powder Pipette (posted 7/15/08)

July 15, 2008
The DryPette®-Varix is a fast, lightweight, hand-held powder pipette that reproducibly, accurately and efficiently dispenses solids and difficult powders.

The new Zinsser DryPette®-Varix is a fast, lightweight, hand-held powder pipette that reproducibly, accurately and efficiently dispenses solids and difficult powders (statically charged materials and other materials that tend to stick). With the DryPette Varix, users can store all important powder handling parameters, such as volume, aspiration and dispense speed, in the electronic controller to guarantee reproducible results.

Reportedly an excellent tool for sample preparation and distribution of almost any dry and powder material from 3 microns, the Zinsser DryPette Varix is available in different sizes from 2 to 565 µl and in larger volumes from 100 to 1900 µl.

For additional information, e-mail Zinsser in Germany at info@zinsser-analytic.com, in the UK at officeuk@zinsser-analytic.com or in North America at info@zinsserna.com.