Royal Crown Derby is using a Compact 900 sieve supplied by Russell Finex in the quality control of the raw materials used in the production of its English Fine Bone China.

Royal Crown Derby, part of the Royal Doulton Group, is using a Compact 900 sieve supplied by Russell Finex in the quality control of the raw materials used in the production of its English Fine Bone China. The company uses the Russell sieve in its slip house, where raw materials are combined to make the clay that forms the basis of all its fine china. Part of a range of high-performance separators, the Compact 900 achieves high throughputs as a result of effective screen evacuation. Material passes straight through the vibratory mesh without hold up to the next process stage. Material is passed through the sieve's vibrating mesh, and is then passed through a second mesh with a slightly larger micron size, which acts as an additional control to protect the virgin material and ensure the quality of the finished product.

For additional information, call (704) 588 9808, fax (704) 588 0738, e-mail sales@russellfinexinc.com or visit http://www.russellfinex.com

Did you enjoy this article? Click here to subscribe to Ceramic Industry Magazine.

You must login or register in order to post a comment.

Multimedia

Videos

Image Galleries

June 2014 Issue Highlights

Our June 2014 issue is now available!

Podcasts

Manufacturing Day 2014

Manufacturing Day organizers share their insights with Managing Editor Kelsey Seidler.

More Podcasts

Ceramic Industry Magazine

CI September 2014 cover

2014 September

You won't want to miss the CI Top 10, traditionally our most popular article of the year!

Table Of Contents Subscribe

THE CERAMIC INDUSTRY STORE

M:\General Shared\__AEC Store Katie Z\AEC Store\Images\Ceramics Industry\handbook of advanced ceramics.gif
Handbook of Advanced Ceramics Machining

Ceramics, with their unique properties and diverse applications, hold the potential to revolutionize many industries, including automotive and semiconductors.

More Products

Clear Seas Research

Clear Seas ResearchWith access to over one million professionals and more than 60 industry-specific publications,Clear Seas Research offers relevant insights from those who know your industry best. Let us customize a market research solution that exceeds your marketing goals.

Directories

CI Data Book July 2012

Ceramic Industry's Directories including Components, Equipment Digest, Services, Data Book & Buyers Guide, Materials Handbook and much more!

STAY CONNECTED

facebook_40px twitter_40px  youtube_40pxlinkedin_40google+ icon 40px