Sacmi has equipped this section of the kiln with heat diffuser tubes, which exchange heat with the product indirectly. Kiln performance has also been improved by splitting the hot air intake piping at the cooling stage.
Savoia chose a configuration where the kiln supervision system has two PCs; these carry out process controls and data management separately.
For more information, visit www.sacmi.com.