Schott: Broadband Erbium-Doped Fiber

March 19, 2002
/ Print / Reprints /
ShareMore
/ Text Size+
Schott recently announced a new broadband erbium-doped fiber, based on its newly developed compact oxide glass, which will provide up to 50% more bandwidth. With this new amplifier medium, Schott has expanded its successful product range of erbium-doped phosphate glasses for planar waveguide amplifiers. The fiber requires significantly less space, enabling more compact designs for amplifiers and telecom equipment. The new amplifier glass material enables shorter fiber lengths, reduced from 15 m to as short as 15 cm for a C-band design. These newly achieved benchmark lengths enable components to consume less space, translating to a significant reduction of the overall system design and assembly costs. Additionally, the new material achieves a wider gain spectrum in the C- and L- bands. In the C-band, for example, the Schott fiber utilizes a gain spectrum up to 50% wider than conventional silica gain media. For an L-band amplifier, efficient amplification can be achieved between 1560 and 1610 nm. In both cases, the gain spectrum is optimized for maximum gain flatness, which requires less filtering and translates into cost savings due to less pumping power needed.

For additional information, call (508) 765-1112, e-mail andreas.zenz@us.schott.com or visit http://www.us.schott.com.

Did you enjoy this article? Click here to subscribe to Ceramic Industry Magazine.

You must login or register in order to post a comment.

Multimedia

Videos

Image Galleries

In-Depth Features

These articles detail innovative advanced ceramic and glass materials and technologies.

Podcasts

Sapphire: An Extreme Performer

Ian Doggett of Goodfellow and CI Editor Susan Sutton discuss the benefits and opportunities provided by industrial sapphire.

More Podcasts

THE MAGAZINE

Ceramic Industry Magazine

CI April 2014 cover

2014 April

Our April issue features details on advanced materials such as ceramic matrix composites and piezoelectric ceramics, among many others. Be sure to check it out!

Table Of Contents Subscribe

THE CERAMIC INDUSTRY STORE

M:\General Shared\__AEC Store Katie Z\AEC Store\Images\Ceramics Industry\handbook of advanced ceramics.gif
Handbook of Advanced Ceramics Machining

Ceramics, with their unique properties and diverse applications, hold the potential to revolutionize many industries, including automotive and semiconductors.

More Products

Clear Seas Research

Clear Seas ResearchWith access to over one million professionals and more than 60 industry-specific publications,Clear Seas Research offers relevant insights from those who know your industry best. Let us customize a market research solution that exceeds your marketing goals.

Directories

CI Data Book July 2012

Ceramic Industry's Directories including Components, Equipment Digest, Services, Data Book & Buyers Guide, Materials Handbook and much more!

STAY CONNECTED

facebook_40px twitter_40px  youtube_40pxlinkedin_40