sp3: Smooth Diamond Coating Service

May 7, 2003
/ Print / Reprints /
ShareMore
/ Text Size+
A new CVD diamond coating service for wear parts has been announced by sp3, Inc. The reactors located in Mountain View, Calif., can provide direct coated, smooth diamond films on flat or shaped wear parts. Recently awarded U.S. patents for both process and product are the cornerstones for this new service. Surface finishes as smooth as 0.1 micron Ra can be routinely obtained on finished parts without the need for post deposition polishing. Wear rates and coefficient of friction are comparable to polished large grain diamond films. Such depositions can be accomplished on a wide variety of materials including most metal carbides, silicon carbides, and either polycrystalline or single crystal silicon.

Did you enjoy this article? Click here to subscribe to Ceramic Industry Magazine.

You must login or register in order to post a comment.

Multimedia

Videos

Image Galleries

April 2014 Issue Highlights

Our April 2014 issue is now available!

Podcasts

Sapphire: An Extreme Performer

Ian Doggett of Goodfellow and CI Editor Susan Sutton discuss the benefits and opportunities provided by industrial sapphire.

More Podcasts

Ceramic Industry Magazine

CI July 2014

2014 July

Our annual Data Book & Buyers' Guide is your best resource for suppliers of materials and equipment for the ceramic, glass, brick and related industries. Check it out!

Table Of Contents Subscribe

THE CERAMIC INDUSTRY STORE

M:\General Shared\__AEC Store Katie Z\AEC Store\Images\Ceramics Industry\handbook of advanced ceramics.gif
Handbook of Advanced Ceramics Machining

Ceramics, with their unique properties and diverse applications, hold the potential to revolutionize many industries, including automotive and semiconductors.

More Products

Clear Seas Research

Clear Seas ResearchWith access to over one million professionals and more than 60 industry-specific publications,Clear Seas Research offers relevant insights from those who know your industry best. Let us customize a market research solution that exceeds your marketing goals.

Directories

CI Data Book July 2012

Ceramic Industry's Directories including Components, Equipment Digest, Services, Data Book & Buyers Guide, Materials Handbook and much more!

STAY CONNECTED

facebook_40px twitter_40px  youtube_40pxlinkedin_40google+ icon 40px