UC Berkeley and LBNL Explore New Materials for Low-Cost Solar Cells (posted 3/9/09)

The study evaluated 23 promising semiconducting materials and discovered that 12 are abundant enough to meet or exceed annual demand.

Unconventional solar cell materials that are as abundant but much less costly than silicon and other semiconductors in use today could substantially reduce the cost of solar photovoltaics, according to a new study from the Energy and Resources Group and the Department of Chemistry at the University of California, Berkeley, and the Lawrence Berkeley National Laboratory (LBNL). These materials, some of which are highly abundant, could expand the potential for solar cells to become a globally significant source of low-carbon energy, the study authors said.

The analysis, which appeared online in the February 13 “Environmental Science & Technology,” examines the two most pressing challenges to large-scale deployment of solar photovoltaics as the world moves toward a carbon neutral future: cost per kilowatt hour and total resource abundance. The UC Berkeley study evaluated 23 promising semiconducting materials and discovered that 12 are abundant enough to meet or exceed annual worldwide energy demand. Of those 12, nine have a significant raw material cost reduction over traditional crystalline silicon, the most widely used photovoltaic material in mass production today.

The work provides a roadmap for research into novel solar cell types precisely when the U. S. Department of Energy and other funders plan to expand their efforts to link new basic research to deployment efforts as part of a national effort to greatly expand the use of clean energy, according to Daniel Kammen, UC Berkeley professor of energy and resources and director of the Renewable and Appropriate Energy Laboratory. Kammen and colleagues Cyrus Wadia, a post-doctoral researcher at LBNL, and A. Paul Alivisatos, interim director of LBNL and UC Berkeley professor of chemistry, embarked on an intensive research project to explore the question of whether high-impact materials have been overlooked or underdeveloped during the last several decades of solar cell research.

“The reason we started looking at new materials is because people often assume solar will be the dominant energy source of the future,” said Wadia, a post-doctoral researcher who spearheaded the research. “Because the sun is the Earth’s most reliable and plentiful resource, solar definitely has that potential, but current solar technology may not get us there in a timeframe that is meaningful, if at all. It’s important to be optimistic, but when considering the practicalities of a solar-dominated energy system, we must turn our attention back to basic science research if we are to solve the problem.”

The most popular solar materials in use today are silicon and thin films made of CdTe (cadmium telluride) and CIGS (copper indium gallium selenide). While these materials have helped elevate solar to a major player in renewable energy markets, they are still limited by manufacturing challenges. Silicon is expensive to process and mass produce. Furthermore, it has become increasingly difficult to mine enough silicon to meet ever-growing consumer demand.

Thin films, while significantly less costly than silicon and easier to mass produce, would rapidly deplete our natural resources if these technologies were to scale to terawatt hours of annual manufacturing production. (A terawatt hour is a billion kilowatt hours.) “We believe in a portfolio of technologies and therefore continue to support the commercial development of all photovoltaic technologies,” Kammen said. “Yet, what we’ve found is that some leading thin films may be difficult to scale as high as global electricity consumption.”

The team identified a large material extraction cost (cents/watt) gap between leading thin film materials and a number of unconventional solar cell candidates, including iron pyrite, copper sulfide and copper oxide. They showed that iron pyrite is several orders of magnitude better than any alternative on important metrics of both cost and abundance. In the report, the team referenced some recent advances in nanoscale science to argue that the modest efficiency losses of unconventional solar cell materials would be offset by the potential for scaling up while saving significantly on materials costs.

Visit http://berkeley.edu for more information.

Links

Did you enjoy this article? Click here to subscribe to Ceramic Industry Magazine.

You must login or register in order to post a comment.

Multimedia

Videos

Podcasts

Thermal Processing Optimization: Using Advanced Rotary Tube Internals

Mike Maggio of Harper International discusses rotary tube internals with Susan Sutton, editor-in-chief.

More Podcasts

THE MAGAZINE

Ceramic Industry Magazine

CI May 2013 cover

2013 May

The 2013 May Ceramic Industry includes articles on treating heat like light, recycling, solar energy, and more. Check it out today!

Table Of Contents Subscribe

THE CERAMIC INDUSTRY STORE

M:\General Shared\__AEC Store Katie Z\AEC Store\Images\Ceramics Industry\handbook of advanced ceramics.gif
Handbook of Advanced Ceramics Machining

Ceramics, with their unique properties and diverse applications, hold the potential to revolutionize many industries, including automotive and semiconductors.

More Products

Clear Seas Research

Clear Seas ResearchWith access to over one million professionals and more than 60 industry-specific publications,Clear Seas Research offers relevant insights from those who know your industry best. Let us customize a market research solution that exceeds your marketing goals.

Directories

0711ci_cover.gif

Ceramic Industry's Directories including Components, Equipment Digest, Services, Data Book & Buyers Guide, Materials Handbook and much more!

STAY CONNECTED

facebook_40px twitter_40px  youtube_40pxlinkedin_40