This company has built an 05-SDM hybrid mill capable of small media milling. The model combines the features of a standard wet -grinding laboratory attritor batch mill with the added benefits of being able to handle small media milling. By adding a specially designed shaft and proprietary Delta Discs, the mill is able to use mini-media from 0.25 to 3 mm and operate at the high shaft speeds (from 300 to 3,000 RPM) required to energize small media.
For additional details, visit www.unionprocess.com.